High efficiency organic antibacterial masterbatch HB104F, ABS flame retardant masterbatch HB119, antibacterial masterbatch HB1042, antistatic masterbatch HB702, PPR functional masterbatch HB2005
  • Film packaging solutions
  • Drink/Flavouring/Daily necessities packaging solutions
  • Pharmaceutical packaging solutions
  • Make-up packaging solutions
  • Thermal forming sheet solutions
  • Injection molding product solutions
  • Product /Material
    Blown Film / LLDPE
    Blown Film / Hdpe
    Cast Film / CPP
    Bopet / BOPP
    Bopet /BOPA
    FAQ & Application Requirements

    1、LLDPE film needs further improvement of transparency.

    2、Preservative film needs to achieve cold/hot anti-frog.

    3、Metal protective film needs to improve adhesive property.

    4、Metal protective film needs anti crystal point and carbon deposition prevention.

    5、Film needs slipping and low surface.

    1、With not enough barrier property, film needs to increase thickness to ensure product shelf life.

    1、The film transparency is not enough.

    2、Serious watermark on high transparent film surface .

    3、Film needs low surface friction coefficient at normal temperature.

    4、Film needs to eliminate thick corona to adjust to high speed packaging.

    5、Film needs low surface friction coefficient at high temperature (80℃, film& metal) to adjust to high speed packaging.

    6、Transparent film needs anti-adhesion.

    7、White film needs to provide high shading light.

    1、The film transparency is not enough.

    2、Film needs low surface friction coefficient at normal temperature.

    3、Film needs to eliminate thick corona to adjust to high speed packaging.

    4、Film needs low surface friction coefficient at high temperature (80℃, film & metal) to adjust to high speed packaging.

    5、Transparent film needs anti-adhesion.

    1、To prevent formation of large spherical crystal and gel, to control broken film, fish eye and spot formation; to prevent adhesion between films, achieving opening improvement of film to adjust high speed printing and packaging; to improve film thickness uniformity and glossiness.

    Solution

    1、To addHB1022 and 1065 into LLDPE to improve transparency of LLDPE film.

    2、To add HB9035 or HB9036 to provide cold/ hot anti-frog ability.

    3、To add HB6660 to improve to improve adhesive property.

    4、To add HB1065 to reduce crystal point, prevent carbon deposition and improve production efficiency.

    5、To add HB7031 to improve open slipping property for LLDPE film.

    1、To add HB1028 to achieve that barrier property of gas and oil could be improved by 20-40% , shelf life could be extended by 50% and film thickness could be reduced by more than 20%..

    1、To add HB6002 and HB8010 to increase transparency and glossiness obviously of CPP casting film.

    2、To add HB8103 to visibly eliminate CPP casting film watermark(water flow).

    3、To add HB1076 to improve slipping and opening of CPP casting film.

    4、To add HB7025 to visibly eliminate CPP casting films static and to be anti-dust.

    5、To add HB9615 to reach COF≤0.2 of film and metal at normal temperature/80℃.

    6、To add HB9043 to eliminate effectively the adhesion between films.

    7、HB370 provides good whiteness, dispersion and hiding power.

    1、To add HB6002 and HB8010 to increase transparency and glossiness obviously of CPP casting film.

    2、To add HB1076 to improve slipping and opening of CPP casting film.

    3、To add HB7025 to visibly eliminate CPP casting films static and to be anti-dust.

    4、To add HB9615 to reach COF≤0.2 of film and metal at normal temperature/80℃.

    5、To add HB9043 to eliminate effectively the adhesion between films.

    1、F-35 multifunctional slipping masterbatch is an essential raw material for BOPA production.

  • Product / material
    PP HDPE
    HDPE
    PP
    FAQ & Application Requirements

    1、The internal and external dimensions of bottle caps with color blue,green, red or yellow are under size.

    2、The cap has big change in size before and after filling drinks with high temperature.

    3、Easy to adhere to mold and hard to remove from mold.

    4、Flavouring bottle cap used frequently is easy to power and wear.

    5、The barrier property of HDPE cap is too low to keep big smell from flavouring.

    6、Lagging equipment,long time for size setting,low production efficiency.

    7、The ring and hinge are easily broken.

    1、 Packaging bottle needs good barrier property to keep smell stored and extend the shelf life.

    1、Packaging material needs to be temperature resistant and anti deformation when steam sterilizing or being filled.

    2、The transparent bottle with liquid needs high toughness and to pass 1.5 m dropping down test after being filled.

    Solution

    1、To add HB1024 to make internal and external dimensions of bottle caps bigger.

    2、To add HB1015 or HB1024 to solve the dimensional variety and tightness problems because of filling drinks with high temperature.

    3、To add HB7030,the speed of removing from mold of bottle cap could be improved greatly.

    4、To add HB7035,the wear resistance and friction coefficient will be improved greatly.

    5、To add HB1028 into HDPE,the barrier property of HDPE cap could be improved by 20-40%.

    6、To add HB1015 or HB1024 to speed up size setting and improve production efficiency greatly.

    7、To add HB6032 to improve tensile elongation and toughness greatly.

    1、To add HB1028 into HDPE to achieve barrier property increased by 20-40%.

    1、To add HB1015, the temperature resistance of PP bottles could be increased by 20-25 degrees.

    2、To add HB6038 into transparent PP to greatly improve toughness and 3L bottle with high transparency passes 1.5 m dropping down test after being filled.

  • Product / material
    Medicament bottle /HDPE
    Syringe/PP
    FAQ & Application Requirements

    1、Packaging material needs barrier property to keep smell stored to ensure the shelf life of medicine.

    1、Products need transparency and dimensional stability.

    Solution

    1、To add HB1028 into HDPE to improve barrier property by 20-40%.

    1、To add HB1035 to improve product transparency and dimensional stability.

  • Product /material
    Make-up bottle cap /PP HDPE
    Make-up bottle/HDPE
    Make-up bottle / PP HDPE
    FAQ & Application Requirements

    1、The post deformation of PP bottle cap is big with unstable size and assembly matching is not good.

    2、The internal and external dimensions of PP\HDPE bottle caps with color blue, green, red or yellow are under size.

    3、Easy to adhere to mold and hard to remove from mold.

    4、Flavouring bottle cap used frequently is easy to power and wear.

    5、Lagging equipment,long time for size setting,low production efficiency.

    1、Packaging bottle needs good barrier property to keep smell stored and ensure the shelf life.

    1、The transparent PP bottle needs high toughness and to pass dropping down test after being filled.

    2、HDPE bottle needs barrier property to ensure the shelf life of medicine.

    Solution

    1、To add HB1015 to reduce post deformation of PP cap, make size stable and improve efficiency of size setting.

    2、To add HB1024 to make internal and external dimensions of bottle caps bigger.

    3、To add HB7030,the speed of removing from mold of bottle cap could be improved greatly.

    4、To add HB7035,the wear resistance and friction coefficient will be improved greatly.

    5、To add HB1015 or HB1024 to speed up size setting and improve production efficiency greatly.

    1、 To add HB1028 into HDPE to achieve barrier property increased by 20-40%.

    1、To add HB6038 into transparent PP to greatly improve toughness and to pass dropping down test after being filled with high transparency.

    2、To add HB1028 into HDPE to improve barrier property by 20-40%.

  • Product /material
    Thermal forming sheet (disposable cup/ lunch-box)/PP
    Functional sheet/ PP
    FAQ & Application Requirements

    1、Thermal forming transparent products need to improve transparency.

    2、hermal forming transparent products need to improve rigidity.

    3、Products need to improve toughening and low temperature resistance.

    4、Products folded need anti-adhesion and opening.

    1、Products need anti-flaming, extrusion and thermal forming.

    Solution

    1、To add HB6002 or HB3810 to improve greatly transparency of cup products.

    2、To add HB6002 to improve rigidity and anti - press strength.

    3、To add HB6032 to improve toughening and low temperature resistance.

    4、To add HB1076 to easily separate the cups or boxes stacked tight.

    1、To add HB1098 to provide PP sheet V0 anti-flaming and good processing performance.

  • Product /material
    High gloss high quality thick-walled product or large size product /PP
    High gloss high quality products /ABS HIPS
    Products with functional requirements /PE PP ABS HIPS
    FAQ & Application Requirements

    1、Long molding cycle, low production efficiency.

    2、Large post deformation, unstable dimension.

    3、Large shrinkage , serious shrinkage mark.

    4、Product rigidity is not enough, too soft.

    5、Product needs to improve surface hardness and scratch resistance.

    6、Product toughness is not enough and needs to enhance impact strength at low temperature.

    7、Product weight is not enough.

    8、The heat resistance temperature of product material is not enough.

    1、Product toughness is not enough with low impact strength so the screw is easy to burst and the drop test fails.

    2、Product UV and weather resistance is bad and yellowing easily.

    3、Product weight is not enough or need to reduce material cost.

    1、Anti-flaming requirement

    2、Antibacterial requirement

    3、Anti-static requirement

    4、Hyper-transparent requirement

    5、Anti-weathering requirement

    Solution

    1、To add HB101 to reduce cooling setting time by 20-40% and improve production efficiency greatly

    2、To add HB101 to eliminate post deformation and improve dimension stability.

    3、To add HB201/HB301/HB803 to solve shrinkage problem when large shrinkage exists.

    4、To add HB101/HB201/HB301/HB803 to improve product rigidity.

    5、To add HB101 to increase product surface hardness.

    6、To add HB603 to enhance product toughness, impact strength at low temperature and transparency.

    7、To add HB201 or HB301 to increase product weight.

    8、To add HB101 to increase PP heat resistance temperature by 20-25℃;

    1、To add HB601 into HIPS products to enhance impact strength and toughness.To add HB602 into ABS products to enhance impact strength and toughness..

    2、To add weather resistance masterbatch HB107 to improve product weather resistance and color stability.

    3、To add HB202 to increase product weight and reduce material cost without influence on glossiness and toughness of high gloss HIPS and ABS.

    1、To add anti-flaming masterbatch HB109 into PP product, additive amount 5% to reach V2 degree, high glossiness, low specific gravity, low precipitation, in conformity with regulations and standards of ROHS and REACH.

    2、Silver ion antibacterial masterbatch HB104, suitable for PE, PP, ABS, HIPS, in line with food sanitary grade, additive amount 4%, sterilizing rate above 90% (11 kinds of normal bacteria)

    3、Anti-static masterbatch HB106 could eliminate product surface static and decrease surface resistance.

    4、Hyper-transparent masterbatch HB103C could highly improve the transparency of homopolymerized PP which could take place of PC by adding HB103C in heat resistant and transparent occasions, thus reducing cost.

    5、Weather resistance masterbatch HB107 could improve product UV resistance and aging resistance.